TEST ITEM | UNIT | ASTM TEST | TYPICAL VALUES |
GAUGE 厚度 | | | 10um | 13.5um | 17um | 22um |
TENSILE | | | | | | |
Tensile Strength (MD) 拉伸强度 | N/mm² | D882 | 130 | 130 | 130 | 125 |
TensileStrength (TD) | 125 | 125 | 125 | 120 |
Elongation(MD) 断裂伸长率 | % | 110 | 115 | 120 | 120 |
Elongation(TD) | 105 | 110 | 110 | 115 |
TEAR 撕裂强度 | | | | | | |
MDat 400gm | g | D1922 | 9 | 14.0 | 16.5 | 22.5 |
TDat 400gm | 9.5 | 13.0 | 18.5 | 23.5 |
SEALSTRENGTH 热封强度 | | | | | | |
MD\HotWire Seal | N/mm | F88 | 0.95 | 1.20 | 1.25 | 1.50 |
TD\HotWire Seal | 1.05 | 1.35 | 1.45 | 1.65 |
COF(Film To Film) | - | | | | | |
Static 静摩擦 | | D1894 | 0.24 | 0.21 | 0.18 | 0.19 |
Dynamic 动摩擦 | | 0.24 | 0.21 | 0.18 | 0.19 |
OPTICS | | | | | | |
Haze 雾度 | | D1003 | 2.2 | 2.4 | 2.6 | 2.9 |
Clarity 透明度 | | D1746 | 98.5 | 98.5 | 98.0 | 98.0 |
Gloss@ 45Deg 光泽度 | | D2457 | 89.0 | 88.5 | 88.0 | 86.5 |
BARRIER 阻隔性 | | | | | | |
OxygenTransmission Rate 透氧率 | cc/㎡/day | D3985 | 12100 | 9700 | 7400 | 6800 |
WaterVapor Transmission Rate 透水气率 | gm/㎡/day | F1249 | 40.5 | 32.5 | 25.5 | 19.5 |
SHRINKAGEPROPERTIES 收缩性 | | MD | TD |
Free Shrinkage 收缩率 | 100℃ | % | D2732 | 19 | 28 |
110℃ | 37 | 45 |
120℃ | 70 | 72 |
130℃ | 81 | 79 |
| | | | MD | TD |
Shrink Tension 收缩张力 | 100℃ | Mpa | D2838 | 2.20 | 2.65 |
110℃ | 2.65 | 3.80 |
120℃ | 2.85 | 4.00 |
130℃ | 2.80 | 3.90 |
MD\Machine Direction TD\Transverse Direction
Note:This information represents our best judgment on the work done, but the company assumes no liability whatsoever in connection with the use of information or findings contained herein.超过相关资料是本工司外部判断之数据报告,未经许可学习。